bare metal? ppg epoxy or etching primer?
9 posts
• Page 1 of 1
Hi, I plan on using ppg's line of products however do they make anything for bare metal such as a etching primer? id like to stick with all the same brand and i havent found anything such as etching or epoxy for bare metal? or could i just use some of that eastwood co etching primer?
|
|
acid etch is old school,......and creates more problems than it solves
use epoxy, if it's PPG: MP170 is a GREAT inexpensive epoxy, and DPLF is the better model, giving more colors, and longer "no need to sand before painting" times either works great on bare metal, and as a final non sanding sealer coat before painting "I believe the state of arkansas flag colors should be,...................PRIMER"
|
|
hi is the epoxy primer used for filling gaos and sading marks ?
or is a primer filler better for that.?? not sure which one to sue either . does epoxy primer spray really thick?? cheer jace |
|
I use the PPG MP170 epoxy primer with the MP175 catalyst. It is part of
PPG Omni system. It a great primer. Bare metal should be sanded 120 to 180, old finishes and body filler 220 to 320. Pick up a product info sheet at your local paint store. Gus |
|
About being thick. I use a 1.4 HVLP and it works great. Gus
|
|
EPOXY is for SEALING off whats underneath, it'll fill minor scratches, say down to about 180 or so, but no, it won't work like a high build urethane 2K primer.
FIller primer, or high build (same thing) is for filling deep scratches say down around 40 grit, and it will spray VERY thick, so you get alot to work with in just a couple of passes PPG calls all epoxies, urethanes, polyesters, sealers AND fillers "primer" so it's a little confusing hope that clears that up "I believe the state of arkansas flag colors should be,...................PRIMER"
|
|
so i can use the ppg stuff as bare metal primer and as sealer before basecoat?
|
|
yes
"I believe the state of arkansas flag colors should be,...................PRIMER"
|
|
Apply PPG MP170 two part epoxy primer over bare steel. Do NOT
sand. If you can see scratches, then apply 2 to 4 coats of MP182 two part surfacer. NOW you sand to smooth out all marks. Then apply basecoat and clear. The MP170 is a great adhisave primer, not a scratch hider. If your metal work is done to the point where it does not show any marks through the MP170 then you dont need the MP182 surfacer.The metal should be sanded 120 - 180 for the MP170. Gus. |
|